| Slit Width [W] (µm) |
0.5 µm |
1.0 µm |
2.0 µm |
4.0 µm |
8.0 µm |
| Slit Length [L] (µm) |
50 |
50 |
50 |
50 |
50 |
| Single Slit Area (µm2) |
25 |
50 |
100 |
200 |
400 |
| Length Spacing [△1] (µm) |
8.5 |
8.5 |
10 |
10 |
10 |
| Width Spacing [△2] (µm) |
3.75 |
8.5 |
8 |
16 |
32 |
| Thickness [t] (µm) |
0.4 |
0.4 |
0.4 |
0.4 |
0.4 |
| Number of Columns |
10 |
10 |
10 |
10 |
10 |
| Number of Rows |
682 |
305 |
290 |
145 |
73 |
| Total Number of Slits / Slot |
6820 |
3050 |
2900 |
1450 |
730 |
| Total Number of Slits / Chip |
20460 |
9150 |
8700 |
4350 |
2190 |
| Porosity (%) |
10.06 |
9.00 |
16.67 |
16.67 |
16.67 |
| Total Open Area / Chip (µm2) |
511500 |
457500 |
870000 |
870000 |
876000 |
Bead Capture Capacities*
| Slit Width [W] (µm) |
0.5 µm |
1.0 µm |
2.0 µm |
2.0 µm (3 µm beads)
|
4.0 µm |
8.0 µm |
8.0 µm (10 µm beads) |
| Total Number of Slits / Chip |
20460 |
9150 |
8700 |
8700 |
4350 |
2190 |
2190 |
| Pore Length (µm) |
50 |
50 |
50 |
50 |
50 |
50 |
50 |
| Total Number of Beads / Pore |
100.0 |
50.0 |
25.0 |
16.0 |
12.0 |
6.0 |
5.0 |
| Total Number of Beads / Chip |
2046000 |
457500 |
217500 |
139200 |
52200 |
13140 |
10950 |
* Unless indicated, the capacities are calculated for spherical beads of the same size as the pore width.