SepCon® Video Protocol: Wetting the membrane
Below is a video protocol for wetting a sepcon device. There is no audio but amounts are detailed.
Below is a video protocol for wetting a sepcon device. There is no audio but amounts are detailed.
I’ve been working over the holiday on trying to make Ag/AgCl electrodes. Here’s the method I’ve come up with so far: 1. 99.99% silver wire is used as the anode (+) and platinum as the cathod (-). 2. Silver wire is coated with chloride in a 1M HCl solution at a constant current of 10…
Following is a written protocol for SEPCON assembly. (Here is a link to a video demonstration) Materials required: wafer tweezers, small sample tweezers (preferably plastic), soft foam board from craft store, wafer of sepcon chips, razor blade, plastic enclosure to store complete SEPCON, top basket, bottom basket, 300 µm thick silicone sheet of pre-cut “U”…
I got some experiences in dealing with cells. This is for your reference. Aseptic Technique and Good Cell Culture Practice Sanitize the cabinet using 70% ethanol before commencing work. Sanitize gloves by washing them in 70% ethanol Put all materials and equipment into the cabinet prior to starting work after sanitizing the exterior surfaces with…
The following procedure is a first draft of the procedure used by Jim and I in an attempt to label BSA with TRITC. This is likely to be updated with photos of the procedure in the future. Prepare reaction buffer by dissolving 1.7g sodium bicarbonate in 200mL of water for a 100mM concentration. Begin to…
We currently use Adobe Illustrator to design silicone gasket geometries for our microfluidic devices. Here is a quick way to do a similar thing from sketchup. The advantage of this procedure is that you can create a complete 3d model of your device and export different snapshots to the 3d printer for bulk fabrication and a…