W502 and 504 Testing

W502 and 504 were tested for burst pressure and air permeability. Only one sample from W502 was tested for burst pressure (the other broke while setting up and I wanted to conserve samples) with a burst pressure of 4.46 psi. The burst pressures for W504 ranged from 2.06 to 6.57 (n=3). Air permeability is shown below.