HUVEC Growth and associated pnc-Si discoloration

HUVEC (P8) growth was monitored over 5 days on different substrates (glass coverslips, tissue culture treated plastic and pnc-Si from W510). The growth curve is as shown below and it can be observed that the growth rate on pncSi in two different trials were observed to be pretty much the same. Decrease in the growth on glass and plastic could be due to initial low density of plating or due to the P8 state of the cells. The division rate of the cells was determined to be: 39.8, 84.8 and 87 hours/division on pnc-Si, glass and plastic respectively.

pnc-Si discoloration was also monitored at respective time points. The samples with cells discolored sooner in comparison to the ones w/o cells. This could be attributed to the waste/byproducts produced by the cells that expedite the discoloration process .