Co-Culture of ADSCs and HUVECs
Scope: Adipose derived stem cells were seeded onto Corning 3um tracketch membranes, human endothelial derived stem cells were seeded onto the membranes approximately five hours later. Numerous control wells were also seeded with ADSCs both on membranes and on the bottom of the 24 well plate. Three days after being seeded, media in each of…