PDMS cell channel repeat
This is an update to my last post, where HUVECs mixed with collagen inside PDMS channels seemed to stay rounded up and not really do much of anything exciting. This time around I made a few adjustments: New collagen protocol – gives 1.5 mg/mL solution before mixing with cells: -10% 10x PBS -1.4% NaOH -38.6%…