Just some quick thoughts about the attached excel on my previous post… The 100K nanosep does not have a hydraulic permeability value at 194.65psi because it passed all 500uL of water through in 1minute which is the smallest interval of time a test can be run at with the new centrifuge. When I get a…
-
-
Hydraluic Permeability Update
I ran some more tests on the microcon and nanosep filtration systems at 21.36psi (4000RPM) and 194.65psi (12,000RPM). Both are rated for forces up to 14,000 time gravity which is about 340psi but after talking to Tom we thought it best to run it at a slightly lower pressure to account for any possible error…