DNA Separations with Controlled Trans-membrane NaCl Gradient
In an attempt to minimize flow due to salt gradients, we ran an experiment in which an intentional gradient was used to set up a slight counterflow from the filtrate to the retentate. This was accomplished by having a 55mM NaCl concentration in the retentate and a 45mM NaCl concentration in the filtrate. The top…