Alexander Shestopalov’s Group Update1: Silane with PEG4 and PEG8 Samples
In this post, I’m going to discuss the results of the different PEG molecular on silane samples. We used same condition to make 4 chips for each sample. And we treat them with BSA, IgG, and PBS to rest the adsorption. We are using the SEM, contact angle and XPS as the testing method. The way we…