Comparitive Functionalization of pnc-Si measured with f-BSA fluorescence intensity
The last of the larger windowless pnc-Si chips were sent to both Adarza and Dr. Shestopalov’s lab for functionalization. Adarza returned chips with PEG-1 and PEG-2 (different rounds of processing) with both 2 hours and 16 hour treatments. They also returned a set treated with an alcohol leaving group ,ethanolamine (EA). They did also supply…