Discoloration in a flipped sample
I am not sure what prompted me to carry out this experiment. I took few samples from W703 (No RTP) and put them in petri dishes with DMEM (-FBS) at room temperature. I had two samples in a dish, with one flipped over (well side up). The sample with well side up discolored much earlier…