Effect of salt on pores (benchtop)
(Transferred from old blog) The above TEM images show that RTP (800C, 5 min) treated samples (from W334) have their pores intact in salt over a period of time! 1M and 2M NaCl solutions were used and TEM samples were taken at different time points. There is some deformation observed near the edges of the…