Desalting BSA: Blank pnc-Si and Mini-Dialysis Units
The ultimate experimental goal of the desalting project is the removal of salts from a salt/protein solution while fractionating certain sized proteins with maximum protein retention and recovery.Thus far we have characterized the flux of salt through our membranes which show flux an order of magnitude greater than cellulose membranes. Our next step is to…