Rapid Prototype of Single Channel Dialysis Device
In order to rapidly test the entire setup for dialysis evaluation, including piezoelectric micro motor and recirculating fluid path, a means of quickly evaluating PDMS designs is needed. A mold was created with a multi-print technique in which printer toner is built up to sufficient height by over printing the same transparency. (see Fig. 1)…