Materials in contact with media in micropump
The pump’s data sheet (located here) describes the pumps materials as:
- polyphenylene sulphone (PPSU)
- polyimide (PI)
- nitrile butadiene rubber (NBR)
It also says that the acceptable particle tolerance is < 50 μm.
This is the info we will need to determine the types of particles we can use with an in-line flow system.