SEM 4 slot 75 nm NPN

SEM of lot # 1208, four-slot 75-nm NPN at 1014x, 1972x, 4101, and 5351x mag.

The next image is with a tilted sample. (from the same lot of chips #1208 4-slot 5.4 mm chips)

The next five show the edge from the top side. I think the second image is the best of the bunch.

The final pair are of the back side of the membranes. I had trouble getting the membranes to break and stick to the glass cover slip. I tried pressure, I breathed on it. I poked at it with tweezers. Any hints will be appreciated.

Scale bars are all 100 nm

 

 

 

Similar Posts

4 Comments

  1. Actually these pores sizes suggest the material is useless for dialysis. We should transfer the membrane onto a slide and image the backside. That is the selective side.

  2. I tried to get backside images but ran out of time, I’m going back in at noon today. I do have blurry images of the backside of the 75-nm wafers and will put them up in the mean time.