Wafer #5244- 0.5 μm Microporous
Manufacturer’s Data
- Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: MPSN 0.5 Microporous
- SKU: MPSN400.C-3LX.1-0.5L1
- Lot Number: 5244
- Quantity Received: 250
- Manufacturer Test Report:
- Pore Size: 530.14 nm
- Flow Data Avg in SLPM
- 2psi: 1.775
- 4psi: 4.483
- 15psi: 16.992
- Burst: 26.083
UR Testing
- Pore size:
- Pore morphology:
- 3 Membranes from this lot were removed for QC measurements
- Chip and Membrane Appearance – (Box-Folder: ).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.
Experiences