Wafer #1519 – 2 Slot Wide NPN

Manufacturer’s Data

  • Delivery Date: 12/8/2023 (picked up and logged by Ahmet Gurcan)
  • Membrane Type: 2 Slot NPN – Wide
  • SKU: NPSN100-2LWM
  • Lot Number: 1519
  • Quantity Received: 177
  • Manufacturer Test Report: Average Porosity: 9.5 %, Average Diameter: 41.4 nm
  • Packing slip & invoice: None

UR Testing

  • Porosity: 14.2% +/- 0.5%
  • Pore size: 58.4 nm +/- 1.7 nm
  • Pore morphology: Standard
  • EDS: N/A
  • Chip and Membrane Appearance:
  • Membrane dimensions (flat surface): 2 x 0.7 mm x 2 mm
  • Full Test Report / Images in Box: See Below for Image:
  • Representative Box Image: See Below

Experiences

  • Cell culture

Similar Posts