Wafer #1524 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 5/20/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100-1L
- Lot Number: 1524
- Quantity Received: 190
- Manufacturer Test Report:
- Pore Size: N/A
- Porosity: N/A
- Flow Data Avg in SLPM
- 2psi: N/A
- 4psi: N/A
- Burst: N/A
- Packing slip & invoice: None
UR Testing
- Porosity: 15.3 +/- 1.4%
- Pore size: 59.9 +/- 2.8 nm
- Pore morphology: 0.83 +/- 0.01 circularity
- EDS: N/A
- Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/sfgo2b7yna2rnyldjhkrri8prv6xctqx ).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.

Experiences
- Cell culture (none as of 5/21/2024)