Wafer #5189 – 0.5 μm Microporous
Manufacturer’s Data
- Delivery Date: 5/20/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: MPSN 0.5 Microporous
- SKU: MPSN400-3L
- Lot Number: 5189
- Quantity Received: 40
- Manufacturer Test Report:
- Pore Size: N/A
- Porosity: N/A
- Flow Data Avg in SLPM
- 2psi: N/A
- 4psi: N/A
- Burst: N/A
- Packing slip & invoice: None
UR Testing
- Porosity:
- Pore size: 485.21 +/- 14.87
- Pore morphology: Rough
- EDS: N/A
- 3 Membranes from this lot were removed for QC measurements
- Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/qqbwrz927n0lnoshcoepia1uchms9a5x).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.
Experiences
- Cell culture (none as of 5/22/2024)