Wafer #240803-20 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 4/14/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100.C-1LZ.0
- Lot Number: 240803-20
- Quantity Received: 220
- Manufacturer Test Report:
- Pore Size: 51 nm
- Porosity: 12%
- Flow Data Avg in SLPM
- 2psi: 0.124
- 4psi: 0.249
- Burst: 5.628 PSI
UR Testing
- Porosity: 10.1%
- Pore size: 51.81 +/- 13.49 nm
- Pore morphology: Standard
- EDS: N/A
- 3 Membranes from this lot were removed for QC measurements.
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- For more information visit: https://rochester.box.com/s/9dco38mtynlwcqx3p8l0shl119tg228j