Wafer #240919-16 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 6/3/2025 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100.C-1LZ.0
- Lot Number: 240919-16
- Quantity Received: N/A
- Manufacturer Test Report:
- Pore Size: 60.3 nm
- Porosity: 17.1%
- Flow Data Avg in SLPM
- 2psi: 0.054
- 4psi: 0.118
- Burst: 7.221 PSI
UR Testing
- Porosity: 4.27%
- Pore size: 50.13 +/- 11.42 nm
- Pore morphology: Standard
- EDS: N/A
- 1 Membrane from this lot were removed for QC measurements.
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- For more information visit: https://rochester.box.com/s/qyjdejddjba3apyr9wqnxq50ppw3eo9c