Wafer #5241- 0.5 μm Microporous
Manufacturer’s Data
- Delivery Date: 7/26/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: MPSN 0.5 Microporous
- SKU: MPSN400.C-3LX.1-0.5L1
- Lot Number: 5241
- Quantity Received: 180
- Manufacturer Test Report:
- Pore Size: 527.48 nm
- Flow Data Avg in SLPM
- 2psi: 2.042
- 4psi: 4.032
- Burst: 29.124
- Packing slip & invoice: None
UR Testing
- Pore size:
- Pore morphology: Smooth
- 3 Membranes from this lot were removed for QC measurements
- Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/nt4fublna46j5g2bhkf8sm7t1q421vpb).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.