Wafer #240803-14 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 12/23/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100.C-1LZ.0
- Lot Number: 240803-14
- Quantity Received: 320
- Manufacturer Test Report:
- Pore Size:
- Porosity:
- Flow Data Avg in SLPM
- 2psi:
- 4psi:
- Burst:
UR Testing
- Porosity: 15.49%
- Pore size: 64.4 +/- 14.62 nm
- Pore morphology: Standard
- EDS: N/A
- 3 Membranes from this lot were removed for QC measurements.
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- For more information visit: https://rochester.box.com/s/dgdh52sp7fvngalekfshxzvyu3gtccw6
Experiences