Author: Ahmet Gurcan

  • Wafer #1514

    Manufacturer’s Data Delivery Date: 11/21/2023 (picked up and logged by Ahmet Gurcan) Membrane Type: 1 Slot NPN SKU: NPSN100-1L Quantity Received: 290 Manufacturer Test Report: Average porosity: 10.3%, Average pore size: 40.2nm Packing slip & invoice: None UR Testing Porosity: N/A (Ran out before report was done) Pore size: N/A (Ran out before report was…