Wafer #1532 – 2 Slot Wide NPN
Manufacturer’s Data Delivery Date: 3/14/2024 (picked up and logged by Ahmet Gurcan) Membrane Type: 2 Slot NPN – Wide SKU: NPSN100-2LWMS Lot Number: 1532 Quantity Received: 299 Manufacturer Test Report: Avg Porosity: 13.4% Avg Pore diameter: 48.7nm Avg flux SLPM at 2PSI: 0.244 Avg flux SLPM at 4PSI: 0.462 Avg Burst Pressure: 6.564 Packing slip…