Wafer #5176 – 2 Slot NPN

Manufacturer’s Data

  • Delivery Date: 1/12/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type: 2 Slot NPN
  • SKU: NPSN100-2LM
  • Lot Number: 5176
  • Quantity Received: 332
  • Manufacturer Test Report:
    • Avg Porosity: 18.3%
    • Avg Pore diameter: 54.9mn
    • Avg flux SLPM at 2PSI: 0.54 PSI
    • Avg Burst Pressure: 3.08 PSI
  • Packing slip & invoice: None

UR Testing

  • Porosity: 21.3 ± 0.6
  • Pore size: 72.5 ± 1.7
  • Pore morphology: Standard
  • EDS: N/A
  • Chip and Membrane Appearance:
  • Membrane dimensions (flat surface): 2 x 0.7 mm x 2 mm
  • Full Test Report / Images in Box: See Below for Image:
  • Representative Box Image: See Below

Experiences

  • Cell culture (none as of 1/16/2024)