Wafer #240803-02 – 1 Slot NPN

Manufacturer’s Data

  • Delivery Date: 12/3/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 1 Slot
  • SKU: NPSN100.C-1LZ.0
  • Lot Number: 240803-02
  • Quantity Received: 40
  • Manufacturer Test Report:
    • Pore Size: 17%
    • Porosity: 57.3 nm
    • Flow Data Avg in SLPM
      • 2psi: .263
      • 4psi: 0.526
      • Burst: 3.557

UR Testing

  • Porosity:
  • Pore size:
  • Pore morphology: Standard
  • EDS: N/A
  • 3 Membranes from this lot were removed for QC measurements.
  • Chip and Membrane Appearance – (Box-Folder: ).
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • Representative membrane Image: See Below.

 