Wafer #1551 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100.C-1LZ.0
- Lot Number: 1551
- Quantity Received: 340
- Manufacturer Test Report:
- Pore Size: 16.5%
- Porosity: 31 nm
- Flow Data Avg in SLPM
- 2psi: 0.1707
- 4psi: 0.192
- Burst: 5.823
UR Testing
- Porosity: 8.78%
- Pore size: 50.01 +/- 15.58 nm
- Pore morphology: Standard
- EDS: N/A
- 3 Membranes from this lot were removed for QC measurements.
- Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/92b3olp03nefgfdqajb62j6ukkl1i6ye).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.