Wafer #240919-18 – 1 Slot NPN

Manufacturer’s Data

  • Delivery Date: 4/29/2025 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 1 Slot
  • SKU: NPSN100.C-1LZ.0
  • Lot Number: 240919-18
  • Quantity Received: 320
  • Manufacturer Test Report:
    • Pore Size: 61 nm
    • Porosity: 18%
    • Flow Data Avg in SLPM
      • 2psi: 0.088
      • 4psi: 0.185
      • Burst: 6.978 PSI