Wafer #5203 – 8 μm Microslit

Manufacturer’s Data

  • Delivery Date: 3/14/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  8-micron microslit
  • SKU: MSSN400-3L-8.0
  • Lot Number: 5203
  • Quantity Received: 102
  • Manufacturer Test Report:
    • Nano Pore Height: 8.022um
    • Avg flux SLPM at 1PSI: 3.272
    • Avg flux SLPM at 2PSI: 4.465
    • Avg flux SLPM at 4PSI: 7.185
    • Avg Burst Pressure: 17.513
  • Packing slip & invoice: None

UR Testing

Experiences

  • Cell culture
    • N/A as of 3/14/2024

Similar Posts