Wafer #1522 – 1 Slot NPN
Manufacturer’s Data
- Delivery Date: 12/20/2023 (picked up and logged by Ahmet Gurcan)
- Membrane Type: NPN 1 Slot
- SKU: NPSN100-1L
- Lot Number: 1522
- Quantity Received: 204
- Manufacturer Test Report: Avg Porosity: 14.2%, Avg Pore diameter: 51 nm, Avg flux SLPM at 2PSI: 0.11 PSI, AVG flux SLPM at 4 PIS: 0.236 PSI, Avg Burst Pressure: 5.74 PSI
- Packing slip & invoice: None
UR Testing
- Porosity: 13.6 +/- 0.9%
- Pore size: 60.1 +/- 2.6 nm
- Pore morphology: Standard
- EDS: N/A
- Chip and Membrane Appearance – (Box Folder: https://rochester.box.com/s/xqx2ub36q7tm5eqdtuwj98cilmsajth7)
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Full Test Report / Images in Box: See Below
- Representative Box Image: See Below


Experiences
- Cell culture (none as of 1/11/2024)