Wafer #5251 – 8 Micron Microslit

Manufacturer’s Data

  • Delivery Date: 8/20/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  8 Micron Microslit
  • SKU: MPSN400.C-3LX.1-8K32
  • Lot Number: 5251
  • Quantity Received: 340
  • Manufacturer Test Report:
    • Flow Data Avg in SLPM
      • 1psi: 6.65
      • 2psi: 9.52
      • 4psi:  14.36
      • Burst: 16.84

UR Testing

  • Slit Width:
  • Slit Length:
  • 3 Membranes from this lot were removed for QC measurements
  • Chip and Membrane Appearance – (Box-Folder: ).
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • Representative membrane Image: See Below.

Experiences

Similar Posts