Wafer #240803-04 – 1 Slot NPN

Manufacturer’s Data

  • Delivery Date: 12/3/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 1 Slot
  • SKU: NPSN100.C-1LZ.0
  • Lot Number: 240803-04
  • Quantity Received: 350
  • Manufacturer Test Report:
    • Pore Size: 17.2%
    • Porosity: 56 nm
    • Flow Data Avg in SLPM
      • 2psi: .161
      • 4psi: 0.336
      • Burst: 3.59

UR Testing

  • Porosity: 15.32.%
  • Pore size: 58.38 +/- 15.11 nm
  • Pore morphology: Standard
  • EDS: N/A
  • 3 Membranes from this lot were removed for QC measurements.
  • Chip and Membrane Appearance – (Box-Folder: https://rochester.box.com/s/fejjpmp2ixi2ipe1u8ecik626qmzbsuh ).
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm