Wafer #1512 – 1 Slot NPN

Manufacturer’s Data

  • Delivery Date: 12/12/2023 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 1 Slot (Square Corner)
  • SKU: NPSN100-1L
  • Lot Number: 1512
  • Quantity Received: 200
  • Manufacturer Test Report: Average Porosity: 10.7%, Average Diameter: 47.6 nm
  • Packing slip & invoice: None

UR Testing

  • Porosity: 15.0 +/- 0.9%
  • Pore size: 61.9 +/- 1.6 nm
  • Pore morphology: Standard
  • EDS: N/A
  • Chip and Membrane Appearance – (Box Folder: https://rochester.box.com/s/wifv7l4jrswfqst3ksxmzk9n5jevn3ww)
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • Full Test Report / Images in Box: See Below
  • Representative Box Image: See Below

Experiences

  • Cell culture (none as of 12/12/2023)
  • Pelin Kasap reported issues with cells going to the center of the membrane after seeding (5/6/2024). Problem is suspected to be related to hydrodynamics and not membrane related issues. The entire membrane is in focus in the image, so tilt in the membrane is unlikely.
  • Chloe (UR) & Dylan (UCOnn) did not have issues that Pelin reported above (5/6/2024)