Cell Suspension, Discoloration and Immunofluorescent assays – Marian
Discoloration Assays Introduction: pnc-Si chips were monitored for discoloration to find chips that had not been previously RTP’d. These assays were necessary in order to find chips that could potentially be used for cell proliferation assays later. Setup: pnc-Si chips were autoclaved and placed in a 24-welled plate with 300uL of DMEM and incubated at…