Wafer #5246- 0.5 μm Microporous

Manufacturer’s Data

  • Delivery Date: 8/16/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  MPSN 0.5 Microporous
  • SKU: MPSN400.C-3LX.1-0.5L1
  • Lot Number: 5246
  • Quantity Received: 200
  • Manufacturer Test Report:
    • Pore Size: 536. 22 nm
    • Flow Data Avg in SLPM
      • 2psi: 1.273
      • 4psi: 3.036
      • 15psi: 13.145
      • Burst: 27.273

UR Testing

  • Pore size:
  • Pore morphology:
  • 3 Membranes from this lot were removed for QC measurements
  • Chip and Membrane Appearance – (Box-Folder: ).
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • Representative membrane Image: See Below.

Experiences