Wafer #5243- 0.5 μm Microporous

Manufacturer’s Data

  • Delivery Date: 8/20/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  MPSN 0.5 Microporous
  • SKU: MPSN400.C-3LX.1-0.5L1
  • Lot Number: 5243
  • Quantity Received: 150
  • Manufacturer Test Report:
    • Pore Size: N/A
    • Flow Data Avg in SLPM
      • 2psi: 1.98
      • 4psi: 4.393
      • 15psi: 17.693
      • Burst: 23.387

UR Testing

  • Pore size: 480.33 nm +/- 2.23 nm
  • Pore morphology: Standard
  • 3 Membranes from this lot were removed for QC measurements
  • Chip and Membrane Appearance – (Box-Folder: ).
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • Representative membrane Image: See Below.