Wafer #240919-19 – 3 μm Dual Scale – Low Porosity

Manufacturer’s Data

  • Delivery Date: 2/5/2025 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 3 micron Dual Scale
  • SKU: DSSN100-1L-3.0-A1 (0.625% Porosity – Not real porosity)
  • Lot Number: 240919-19
  • Quantity Received: 70
  • Manufacturer Test Report:
    • Average Porosity (nanoporosity):
    • Average Diameter (microporous):
    • Average Diameter (nanoporous):
    • Average Flux @ 1 PSI:
    • Average Flex @ 2 PSI:
    • Average Burst Pressure (PSI):
  • Packing slip & invoice: None

UR Testing

  • Average Porosity (nanoporosity): 11.54%
  • Average Porosity (microporoisty):
  • Pore Size (nanopores): 60.32 +/- 15.87 nm
  • Pore Size (micropores):
  • Pore morphology: Standard
  • EDS: N/A
  • Chip and Membrane Appearance:
  • Membrane dimensions (flat surface): 0.7 mm x 2 mm
  • For more information visit: https://rochester.box.com/s/5a8fkrj935lef3j0fv55f8oy1qccbznx

 