Wafer #1510- 2 Slot NPN Standard

Manufacturer’s Data

  • Delivery Date: 10/8/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type: 2 Slot NPN – Standard
  • SKU: NPSN100-2L
  • Lot Number: 1510
  • Quantity Received: 220
  • Manufacturer Test Report:
    • Avg flux SLPM at 2PSI: 0.301
    • Avg flux SLPM at 4PSI: 0.606
    • Avg Burst Pressure: 5.919
    • Average porosity: 14.9%
      Avg pore size: 52.9 nm
  • Packing slip & invoice: None

 

UR Testing

Experiences

  • Cell culture
    • N/A as of 10/8/2024