High School Conductivity Project
Two high school students, Nick and Nikita, were supervised to study the effects our Sepcon membranes had on potential charge based separations. Using standard 30 nm cutoff Sepcons and the pressure cell, they performed a set of experiments with high (1 M) and low concentration (100 mM) KCl. They measured the conductivity of the filtrate…