A closer look at separations
UPDATED 12/12/07 – Added data on albumin. In these gels, the band from beta-galactosidase appears to overlap with phosphorylase b making it difficult to determine which protein passes and which is retained. I have used Mike Bindschadler’s pore imaging software to find the pore sizes of the three membranes I have use to perform succesful…