CB Report Update
Today I looked at 3 more wafers:
w158 (9/7/07) – some pinholes, overwhelming amount of very fine debris, not cbs as far as I can tell
w160 (9/7/07) – some pinholes, debris, no cbs
w171 (9/26/07) – many pinholes, lots of debris, no cbs
Link to updated report.