Test of Theory– Can we successfully bind Human IgG to the protein A beads and then remove it with buffer B?

Test of Binding/ Unbinding (Carrie and Barrett): Test to see if we can successfully bind Human IgG to the protein A beads and then remove it with buffer B.

After ordering the new human IgG and protein A beads, I have been working on a higher-quality analysis of the binding and dissociating of the IgG and the beads.

Use “Protein A Beads and IgG Binding and Filtering (with SepCon Format)”

9/23/09: Swell Protein A Beads in Buffer A. Add Human IgG.

Swell Beads:

  • Added 200μl of buffer A. The mixture was very dry.
  • Added an additional 200μl, but it was still very dry.
  • Added 200μl more. The mixture was a slurry, but a very thick one with the beads crusting onto the walls and cap of the conical.
  • Added 400μl. The slurry was still very thick and the beads were not staying in solution
  • Add more buffer. Total volume= 11 ml.

Store in 20% ethanol.

9/24/09

1) Rinse beads with Buffer A to remove ethanol.

2) Add human IgG to the beads.

    9/25/09

    1) Rinse with Buffer A to get rid of any unbound IgG (rinse until obtain a neutral Bradford Assay reading).

    Bradford Assay:

    • 2×10μl blank samples (Buffer A) [B1&2]
    • 2×10μl samples after initial spin-down (unbound IgG) [B3&4]
    • 2×10μl after 1 rinse [B5&6]
    • 2×10μl after 2 rinse2 [B7&8]
    • 2×10μl after 3 rinses [B9&10] (B7 had a few beads in solution)

    –> All appear light brown. This is good because it means that there is very little unbound IgG in solution.

    2) Try to unbind IgG from beads with buffer B.

    • Add 1mL of buffer B (at pH 4). Mix for 15 minutes at room temperature; spin for 2 minutes at 1500 rpm.
    • Add 59 μl of 1M NaOH, to neutralize the pH of buffer B.
    • Take 2×10μl for protein assay [A5&A6] –> When add dye, well is light brown. If the IgG had come off the beads, it should be blue.

    3) Try to unbind IgG again.

    • Add 1mL of buffer B. Mix for 15 minutes at room temperature; spin for 2 minutes at 1500 rpm.
    • Transfer 1 mL to a new tube and add 59μl of 1M NaOH.
    • Take 2×10μl for protein assay [A7&8]. –> Still seems like no IgG is coming off.
    • [A9&10] –> Buffer B, to have a blank to compare the other results to.

    4) Try again, but mix for 30 minutes.

    • Add 1mL of buffer B. Mix for 30 minutes at room temperature; spin for 2 minutes at 1500 rpm.
    • Transfer 1 mL to a new tube and add 59μl of 1M NaOH.
    • Take 2×10μl for protein assay [C1&2].

    –> Still seems like no IgG is coming off

    5) New attempt: Make buffer B at pH 3 and repeat elution [C3&4]; mix for 30 minutes.

    • It worked!!!!
    • [B11&12]–> New Buffer B (blank)

    6) Finishing steps:

    • Do 1 more elution to see if any more IgG–> Still IgG
    • Do 1 last elution (2 hours) to remove all of IgG from beads
    • Take 2×10μl sample [D1&2]
    • Do protein assay
    • Still a bit high ABS
    • Rinse beads in 20 RV of Buffer A (~7 spins of 1.5mL)
    • Store beads in 20% ethanol/ 80% Buffer A

    TECAN readings:

    <> 1 2 3 4 5 6 7 8 9 10
    A blank (buffer A) After protein A bead+ IgG spun down after 1 rinse with Buffer A after 2 rinses with Buffer A after 3 rinses with Buffer A
    B 0.2113 0.2157 0.2183 0.209 0.2189 0.2077 0.2102 0.2103 0.2484 0.2015
    C
    Elution
    Buffer B Elution 1 Elution 2 Elution 3
    0.2095 0.2027 0.2429 0.2492 0.2088 0.2039 0.2338 0.2238
    Change to pH 3 elution buffer
    new Buffer B Elution 1 Elution 2 2 Hour Elution
    0.1963 0.2019 0.3637 0.3754 0.2968 0.3022 0.2309 0.2367

    Similar Posts