I constructed a plot of hydraulic permeability based on the flow rates that Sterlitech has predicted for their membranes.

Looking at the permeability values that I posted last week, outside the tested that appeared to leak, there was a 0.01um membrane with a permeability of 33.4, two 0.05um membranes with permeabilities of 59.9 and 71.1, and a 0.10um membrane with a permeability of 262.4.