Wafer #5252 – 8 Micron Microslit
Manufacturer’s Data
- Delivery Date: 8/20/2024 (picked up and logged by Ahmet Gurcan)
- Membrane Type: 8 Micron Microslit
- SKU: MPSN400.C-3LX.1-8K32
- Lot Number: 5252
- Quantity Received: 340
- Manufacturer Test Report:
- Flow Data Avg in SLPM
- 1psi: 5.077
- 2psi: 7.325
- 4psi: 10.608
- Burst: 12.384 nm
- Flow Data Avg in SLPM
UR Testing
- Slit Width:
- Slit Length:
- 3 Membranes from this lot were removed for QC measurements
- Chip and Membrane Appearance – (Box-Folder: ).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.