Wafer #240803-06 – 2 Slot NPN

Manufacturer’s Data

  • Delivery Date: 12/18/2024 (picked up and logged by Ahmet Gurcan)
  • Membrane Type:  NPN 2 Slot
  • SKU: NPSN100-2LWMS
  • Lot Number: 240803-06
  • Quantity Received: 170
  • Manufacturer Test Report:
    • Pore Size: 53.5
    • Porosity: 15.5
    • Flow Data Avg in SLPM
      • 2psi: 0.366
      • 4psi: 0.641
      • Burst: 4.003

UR Testing

  • Porosity: 14.35%
  • Pore size: 50.85 +/- 13.42 nm
  • Pore morphology: Standard
  • EDS: N/A
  • 3 Membranes from this lot were removed for QC measurements.
  • Chip and Membrane Appearance – (Box-Folder: ).
  • Membrane dimensions (flat surface): 2 x (0.7 mm x 2 mm)
  • For more details visit: https://rochester.box.com/s/x2f6nvjavku8s41qylwm66k9rulwy3lz

 