Fibroblasts spreading on glass

I carried out another trial of spreading experiments and following time lapse movies show the spreading of fibroblasts on glass ( @ 37C, in L15 media supplemented with 10% FBS) over a time period of ~7 hrs.

Fibroblast spreading on glass 1

Fibroblast spreading on glass 2

Time lapse movies for fibroblasts spreading on pncSi are on their way.