Zeta Potential Measurements of Microbeads

I tested all the microbeads that the Gaborski and Lapizco-Encinas labs own.  The results are summarized below.  The sizes ranged from 50 nm to 2 µm.  I mixed them to concentrations of 0.2 g/L for all bead less than 1 µm and 1.0 g/L for all 1 µm or greater.  Interestingly, the scans look rather poor for all the samples at 1 µm or larger.  I plan to repeat a couple at higher concentration to see if this helps.

 