Wafer #240701-05 – 1 Micron Microslit
Manufacturer’s Data
- Delivery Date: 8/25/2025 (picked up and logged by Ahmet Gurcan)
- Membrane Type: 1 Micron MicroSlit
- SKU: MSSN400.C-3LX.1-1.0E2
- Lot Number: 240701-05
- Quantity Received: 250
- Manufacturer Test Report:
- Flow Data Avg in SLPM
- 1psi: 1.83
- 2psi: 3.47
- 4psi: 6.34
- 15psi: 15.6
- Burst: 26.99
- Flow Data Avg in SLPM
UR Testing
- Slit Width:
- Slit Length:
- 3 Membranes from this lot were removed for QC measurements
- Chip and Membrane Appearance – (Box-Folder: ).
- Membrane dimensions (flat surface): 0.7 mm x 2 mm
- Representative membrane Image: See Below.
Experiences